Calculated influences of starting materials composition on carbothermal nitridation synthesis of silicon nitride/silicon carbide composite powders

Jinwang Li,Jiemo Tian,Limin Dong
DOI: https://doi.org/10.1023/A:1017551419640
IF: 4.5
2001-01-01
Journal of Materials Science
Abstract:Equilibrium phase composition at 1 atm total pressure is quantitatively calculated as the function of starting materials composition for carbothermal nitridation synthesis of Si 3 N 4 /SiC composite powders. N 2 flow is simulated by the N 2 amount in the starting materials. At low starting N 2 content (molar ratio N 2 /SiO 2 ≤ 100), Si 3 N 4 and SiC can not exist in equilibrium at the same temperature. At higher starting N 2 content, the Si 3 N 4 -SiC coexisting temperature range appears above 1760 K. The upper limit of the temperature range becomes higher with increasing starting N 2 content. Starting carbon content affects the composition in the equilibrium powder products. The calculation results are compared with experiments.
What problem does this paper attempt to address?