Abstract:The sub-micron sized Sc2O3 doped tungsten powders with the particle size distributed from 500 to 1 100 nm have been fabricated by Sol-Gel methods combined with two-step hydrogen reduction process.The W-Sc2O3 targets have been sintered via spark plasma sintering(SPS) using the obtained sub-micron sized powders pre-treated under different conditions.The comparative density,rockwell hardness,and surface morphology have been studied in this paper.Results indicate that the W-Sc2O3 targets have been successfully sintered at 1 300 ℃ with the sub-micron sized powders,whose sintering temperature is much lower than that of using micrometer sized powders.The sintered W-Sc2O3 targets with uniformly distribution of Sc have a highly comparative density of 96.4% and rockwell hardness of 86.4 HRC.