Effects of Preparation Conditions on the Structural and Optical Properties of Spark Plasma‐Sintered PLZT (8/65/35) Ceramics

YJ Wu,J Li,R Kimura,N Uekawa,K Kakegawa
DOI: https://doi.org/10.1111/j.1551-2916.2005.00601.x
IF: 4.186
2005-01-01
Journal of the American Ceramic Society
Abstract:Transparent lanthanum‐doped lead zirconate titanate (PLZT) ceramics with high density were fabricated using spark plasma sintering (SPS), a recently developed hot‐pressing method. A wet–dry combination method was used to prepare the fine PLZT powders. The average grain size of the PLZT ceramics was less than 1 μm, because of a relatively low sintering temperature and a very short sintering time. The transmittance of PLZT ceramics increased with an increase of calcination temperature up to 700°C and then it slightly decreased with further increase of calcination temperature. The transmittance strongly depended on the SPS temperature and heat‐treatment temperature. The pellet sintered at 900°C for 10 min and heat treated at 800°C for 1 h with a thickness of 0.5 mm showed a transmittance of 31% at a wavelength of 700 nm. The relationships between the transmittance and the microstructure were investigated.
What problem does this paper attempt to address?