Abstract:<p>Ceramic/metal composites, as high-temperature structural materials, have limited applications because of their poor machinability. AlN/Mo/Mo<sub>2</sub>B machinable composites were fabricated by adding h-BN to AlN/Mo composites by plasma-activated sintering at various temperatures and at an axial pressure of 30 MPa under argon atmosphere. The sample sintered at 1500 °C exhibited excellent machinability for cemented carbide tools, with a bending strength of approximately 500 MPa and a Vickers hardness value of 9.34 GPa. The effects of sintering temperature on the microstructure, mechanical properties, and machinability were investigated, and the reactions introduced by adding h-BN were studied. These reactions reinforced the composite and newly introduced a Mo<sub>2</sub>B phase, which showed better ability to deflect cracks and prevent them from moving deep inside the composite, thus improving its machinability. This research provides a possible solution for improving the machinability of ceramic/metal composites without sacrificing the strength.</p>
materials science, ceramics
What problem does this paper attempt to address?