Recovery lithium and potassium from lepidolite via potash calcination-leaching process

Yuqing Kuai,Wengui Yao,Hongwen Ma,Meitang Liu,Yuan Gao,Ruoyu Guo
DOI: https://doi.org/10.1016/j.mineng.2020.106643
IF: 5.479
2021-01-01
Minerals Engineering
Abstract:<p>A new comprehensive way to extract lithium and potassium from lepidolite through calcination process with the additive of K<sub>2</sub>CO<sub>3</sub> has been proposed. By using flowing water vapor, the lepidolite concentrate mixed with 58.5% of K<sub>2</sub>CO<sub>3</sub> could generate acid-soluble potassium aluminum silicate (KAlSiO<sub>4</sub>) and water-soluble lithium/potassium silicate (Li<sub>2</sub>SiO<sub>3</sub>/K<sub>2</sub>SiO<sub>3</sub>) at 850 °C for 2 h. Additionally, 80% of fluorine could be removed. The reaction feasibility between lepidolite ore and K<sub>2</sub>CO<sub>3</sub> was firstly evaluated through thermodynamic calculation. The decomposition mechanism was explored through XRD and TG-DSC analysis. The experimental results reveal that the decomposition of lepidolite undergoes following phase transformation: trilithionite phase → lepidolite phase → KAlSi<sub>2</sub>O<sub>6</sub> → KAlSiO<sub>4</sub>. As the desilication process proceeds, silicon is given off and forms lithium/potassium silicate. Through a water leaching process, soluble Li<sub>2</sub>SiO<sub>3</sub>/K<sub>2</sub>SiO<sub>3</sub> could be separated from KAlSiO<sub>4</sub>. The extraction efficiency of Li and K could severally reach 95.52% and 95.70% from soluble silicates through water leaching process, under the optimum conditions. Then the residue KAlSiO<sub>4</sub> could be easily recovered by acid solution. This new technique for processing lepidolite could make most of all of its components, as well as being environmentally friendly.</p>
engineering, chemical,mining & mineral processing,mineralogy
What problem does this paper attempt to address?