Structural features and thermoelectric performance of Sb- and Bi-doped Cu2SnSe3 compounds

Shu-Ping Deng,Xian-Yan Jiang,Li-Li Chen,Zi-Ye Zhang,Ning Qi,Yi-Chu Wu,Xin-Feng Tang,Zhi-Quan Chen
DOI: https://doi.org/10.1007/s12598-021-01724-1
IF: 6.318
2021-04-17
Rare Metals
Abstract:<span class="a-plus-plus abstract-section id-a-sec1 outputmedium-all"><p class="a-plus-plus">In this paper, a series of Sb-doped and Bi-doped Cu<sub class="a-plus-plus">2</sub>Sn<sub class="a-plus-plus">1-<em class="a-plus-plus">x</em></sub>M<sub class="a-plus-plus"><em class="a-plus-plus">x</em></sub>Se<sub class="a-plus-plus">3</sub> samples (M = Sb, Bi) are prepared by vacuum melting combined with the spark plasma sintering process. The effects of different atomic doping amounts on their properties are discussed. Structural studies indicate that all obtained samples comprise a single Cu<sub class="a-plus-plus">2</sub>SnSe<sub class="a-plus-plus">3</sub> phase. Sb and Bi atoms are experimentally demonstrated to be efficient cation dopants for increasing the transport performance. Compared with that doping on the cation site, Bi doping is much more efficient in increasing the electron concentration of the Cu<sub class="a-plus-plus">2</sub>SnSe<sub class="a-plus-plus">3</sub> system. Ultimately, a high figure of merit of 0.36 is achieved in the Cu<sub class="a-plus-plus">2</sub>Sn<sub class="a-plus-plus">0.94</sub>Sb<sub class="a-plus-plus">0.06</sub>Se<sub class="a-plus-plus">3</sub> sample at 773 K due to the enhanced power factor and lowered lattice thermal conductivity, which are 1.73 times higher than those of the pure sample. Our results provide an efficient approach to enhance thermoelectric performance via other doping atoms, which could also be applied to copper-based chalcogenide materials.</p></span>
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?