Abstract:<p>SiC ceramics were sintered with Mg<sub>2</sub>Si and Ni<sub>3</sub>Al additives at 900–1300 °C. Densification was achieved at temperatures as low as 1300 °C, and the microhardness and fracture toughness were significantly improved from 4.95 GPa to 8.17 MPa m<sup>1/2</sup> for the ceramic without Ni<sub>3</sub>Al to 13.59 GPa and 10.40 MPa m<sup>1/2</sup> for the ceramic sintered with 10 wt% Ni<sub>3</sub>Al, representing improvements of 174.55% and 27.29%, respectively. Some of the Ni<sub>3</sub>Al was converted into Ni with a (110)<sub>Ni3Al</sub> || (002)<sub>Ni</sub> crystal morphology, and the SiC bonded to Ni<sub>3</sub>Al with a (103)<sub>SiC</sub> || (112)<sub>Ni3Al</sub> crystal morphology. These well-matched crystal morphologies led to perfect lattice coherence. The Ni-rich regions prevented the elongation of cracks, resulting in improved fracture toughness.</p>
materials science, ceramics
What problem does this paper attempt to address?