Chromium doped tungsten alloy for plasma-facing components of fusion reactors formed by compression plasma flows

S Al Mazrouei,A Mohanta,V I Shymanski,G Matras,C Kasmi
DOI: https://doi.org/10.1088/1742-6596/2368/1/012025
2022-11-12
Journal of Physics: Conference Series
Abstract:Chromium doped tungsten (Cr-W) alloys are formed by compression plasma flows (CPFs) treatment at different absorbed energy densities (20 – 50 J/cm 2 ), and are characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive X-ray microanalysis (EDX), and the Vickers hardness test. XRD analysis betokens that the dominant crystal orientation changes from (110) to (200) after CPFs treatment, and the intensity ratio (I 200 /I 110 ) between the diffraction lines corresponding to (200) and (110) planes increases with an increase in the absorbed energy density. SEM and EDX analyses betoken spatial inhomogeneity at 20 J/cm 2 , improved uniformity at 30 J/cm 2 , and cracks at higher energy density. The hardness of the Cr-W alloy varies with absorbed energy density and has a maximum value of 379 HV at 20 J/cm 2 .
What problem does this paper attempt to address?