Ductility deterioration induced by L2 1 phase in ferritic alloy through Ti addition

Xu Chen,Shaowen Peng,Ye Liu,Song Bai,Lin Zhang,Shuang He,Oleg I. Gorbatov,Xuanhui Qu
DOI: https://doi.org/10.1016/j.jmrt.2023.06.176
IF: 6.267
2023-06-29
Journal of Materials Research and Technology
Abstract:Ductility deterioration induced by L2 1 -Ni 2 AlTi precipitates in the aged ferritic alloys was examined systematically by using a combination of scanning transmission electron microscope (STEM), mechanical tests and first-principles thermodynamic calculations. The experimental studies revealed that the strength and hardness of the aged Fe–10Cr–5Ni–1Al–1Ti ferritic alloy containing B2–NiAl and L2 1 -Ni 2 AlTi precipitates were higher than that of the aged Fe–10Cr–5Ni–1Al ferritic alloy containing NiAl precipitates, whereas the elongation-to-failure decreased dramatically from 9.3% to 0.3% indicating an obvious ductility deterioration due to the formation of L2 1 -Ni 2 AlTi precipitates. This was also confirmed by the observation of fracture transition mode from dimpled failure to cleavage failure. The first-principles calculations, concerning the precipitate/matrix interface, were carried out to provide a theoretical analysis for the ductile–brittle transition by means of empirical ductility criteria ratios G/B and (C12–C44)/B as well as cleavage energy. The cleavage energy results indicated an intrinsic brittleness of the L2 1 -Ni 2 AlTi phase and the L2 1 -Ni 2 AlTi/BCC-Fe interface. Our analysis revealed that the intrinsic brittleness of L2 1 -Ni 2 AlTi phase and L2 1 -Ni 2 AlTi/BCC-Fe interface plays a vital role in determining the deformation behavior of the aged Fe–10Cr–5Ni–1Al–1Ti alloy.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?