Abstract:Fe-30%Cu(mass fraction) and Sn,Cu powders were used as matrix materials of diamond saw blades with additives of W/Cr/Ni and WC/Cr3C2/Ni,respectively.The diamond saw blades were prepared by compression sintering.The relative density and mechanical properties of the matrix materials and the cutting ability of the diamond saw blade were investigated.The results show that the hardness,impact toughness and transverse rupture strength increases by 19.2%,11.7% and 6.9%,respectively,while the relative density of the matrix materials decreases from 96.50% to 93.09%~94.78% after adding W/Cr/Ni and WC/Cr3C2/Ni.The best properties of dry cutting of the diamond saw blades are obtained when the volume of W is 2.44% and the volume of Cr is 2.44%.The abrasive ratio and cutting velocity is 105.3 m/mm and 1.66 m/min,respectively.The best properties of wet cutting of the diamond saw blades are obtained when the volume of WC is 4.36% and the volume of Cr3C2 is 0.67%.The abrasive ratio and cutting velocity is 109.6 m/mm and 2.17 m/min,respectively.
What problem does this paper attempt to address?