High Temperature Oxidation and Tribological Behavior of Cr3C2-25CoNiCrAlY and Cr3C2-25NiCr Coatings Prepared by AC-HVAF

Zhou Xiao-long,Zeng De-chang,Wang Gang,Zhang You-sheng
DOI: https://doi.org/10.11933/j.issn.1007-9289.20170214001
2017-01-01
China surface engineering
Abstract:To improve the high temperature oxidation and wear resistance of hot working dies, Cr3C2-25CoNiCrAlY and Cr3C2-25NiCr coatings were prepared by activated combustion high velocity air fuel (AC-HVAF) spraying on H13 steel, respectively. The high temperature oxidation and wear resistance performances of the coatings were contrastively studied. The microstructure and phase structure were investigated by SEM, EDS and XRD. The results show that the Cr3C2-25CoNiCrAlY coating provides superior high temperature oxidation resistance compared with the Cr3C2-25NiCr coating. The oxidation weight gain of Cr3C2-25CoNiCrAlY coating (0.80 mg/cm(2)) is less than that of the Cr3C2-25NiCr coating (0.87 mg/cm(2)) after cyclic oxidation at 800 degrees C for 100 h, which is attributed to the formation of the denser oxidation layer and spinel phase with excellent high temperature stability on surface of the Cr3C2-25CoNiCrAlY coating. The Cr3C2-25CoNiCrAlY coating has lower friction coefficient and wear rate than that of the Cr3C2-25NiCr coating at 700 degrees C due to the.-matrix phase (Co-Ni-Cr solid solution) in the Cr3C2-25CoNiCrAlY coating having great high temperature strength and thermal fatigue properties, which is better supportive for carbide hard phase and enhances the spalling resistance of the coating.
What problem does this paper attempt to address?