Recrystallization behavior of pure tungsten with different rolling ratio during isothermal annealing at temperature range of 1250-1350 ℃

YU Ming,WANG Kang,ZAN Xiang,LUO Lai-ma,WU Yu-cheng
DOI: https://doi.org/10.13289/j.issn.1009-6264.2017-0089
2017-01-01
Abstract:Isothermal annealing experiments of pure tungsten at 1250,1300 and 1350 ℃ with rolling ratio of 50% (W50),67% (W67) and 90% (W90) were carried out.The effects of annealing temperature and rolling ratio on recrystallization process of the pure tungsten were investigated by means of micro-hardness test and microstructure analysis.The results show that the recrystallization activation energies of the W50,W67 and W90 are 478,496 and 447 kJ/mol respectively fitted by Arrhenius relation.The service lives of the W50,W67 and W90 are predicted to be 172.7,72.3 and 8.5 years at 900 ℃.Based on the statistical analysis of the recrystallized grains of the pure tungsten samples after isothermal annealing at 1350 ℃,it is found that the average grain size after the complete recrystallization decreases with the increasing of the rolling ratio.
What problem does this paper attempt to address?