Abstract:When Shenmu coal of high calcium and sulfur content is fired in a 1025t/h pulverized coal fired boiler, the auto-sulfur retention efficiency gets as high as 27%~33% under 100% load. About 60% of the minerals and calcium ingredients fed into the furnace turned into fly ash, and less than 10% remains in the bottom ash. About 70% of the sulfur entering the furnace is discharged together with the flue gas in form of gaseous SO_2, less than 10% fixed by the fly ash, and less than 1% fixed by the bottom ash. It is found by XRD analysis that the content of the quasi glass-like phase, formed under the high temperature is found to be much higher in the fly ash than in the bottom ash. The fly ash also contains the sulfur auto-retention product CaSO_4 and cristal phase CaO which has not taken part in the reaction, but they not to be detected in the bottom ash, but which was found to contain quite a lot of newly formed cristal phase albite.Figs2,tables7 and refs4.
What problem does this paper attempt to address?