Microstructures of Self-Desulfurization Residue of Shenmu Coal Ash in Combustion

程军,周俊虎,徐小琼,刘建忠,曹欣玉,岑可法
DOI: https://doi.org/10.3969/j.issn.0253-2409.2004.06.010
2004-01-01
Abstract:The sulfur-retention properties and microstructures of Shenmu coal ash are studied. It is found that the self-desulfurization efficiency of Shenmu coal with an initial molar ratio Ca/S of 1.45 dramatically decreases from 63.5% to 6.4%, when the furnace temperature increases from 800?℃ to 1?200?℃. The reason is that the active calcium (CaCO_3 and CaO) content is 22.4% to give a sulfation product CaSO_4 content of 18% in the combustion residue at 800?℃. It is composed of many small particles with fine pores (specific surface area of 4.6?m~2·g~(-1) and mean pore diameter of 14.2?nm), which form a loose cotton-like structure and provide large surface area for sulfation reaction. But none of the phases of CaCO_3, CaO and CaSO_4 is found in the coal ash at 1?200?℃. It is composed of many large nonporous particles with smooth surfaces (specific surface area of 2?m~2·g~(-1) and mean pore diameter of 5.5?nm), due to the high levels of sintering swell and melting.
What problem does this paper attempt to address?