2005-01-01
Abstract:In order to better utilize FBC solid residues, the microstructures of two Chinese coal ashes derived from combustion at 800 degrees C are studied. The initial Ca/S of 1.45 in Shenmu coal is higher than that of 1.07 in Huangling coal. Therefore, the active calcium and sulfation product contents in Shenmu coal ash are higher than those in Huangling coal ash. With the specific surface areas of 4.59-12.27 m(2)/g and mean pore diameters of 114-142 angstrom, both of the coal ashes can provide necessary gas diffusion channels. There are many loose cotton-like structures in Shenmu coal ash, which are probably the shells of sulfation product CaSO4 covering the CaCO3 particles.