CexTi1-xO2 mixed oxides supported CuO catalyst for NO reduction by CO

LP Lou,XY Jiang,YX Chen,GL Lu,RX Zhou,XM Zheng
IF: 4.632
2003-01-01
Journal of Rare Earths
Abstract:CexTi1-xO2 mixed oxides of different mole ratios (x=0, 0.1, 0.2similar to0.9, 1.0) were prepared by co-precipitation of TiCl4 with Ce(NO3)(3) and then loaded with different amounts of CuO. The effects of CuO on NO+CO reaction were investigated, and the structure and reductive properties of various CuO/CexTi1-xO2 were characterized by the methodologies of BET, TPR and XRD. The results show that different Ce/Ti mole ratios and calcination temperatures induce changes of structure and reductive properties of the CexTi1-xO2 mixed oxides. When x=0.1similar to0.5, amorphous CeTi2O6 phase mainly forms at 650degreesC compared to the formation of CeTi2O6 which crystallizes at 800degreesC. When x>0.6, some TiO2 enters the CeO2 lattice and a CeO2-TiO2 solid solution is formed. The activity of 6%CuO/CexTi1-xO2 calcined at 650degreesC is largely affected by the x values, which is the highest when x=0.3, 0.4 and 0.9. The NO conversion reaches 70% at a reaction temperature of 150degreesC. By comparison, the x values have little effect on the activity of 6%CuO/CexTi1-xO2 calcined at 800degreesC. There are strong interactions between CuO and CeTi2O6, i.e., formation of the CeTi2O6 phase shifts the CuO reduction peak temperature from 380 to 200degreesC, and CuO, in turn, shifts the CeTi2O6 reduction peak temperature from 600 to 300degreesC.
What problem does this paper attempt to address?