Correlation of Deactivation of Ni-Mo-W/Al2o3 During Ultra-Low-Sulfur Diesel Production with Surface Carbon Species

Zhang Le
2017-01-01
Abstract:The deactivation of a Ni-Mo-W/Al2O3 catalyst during ultra-low-sulfur diesel production was investigated in a pilot plant. The reasons of catalyst deactivation were analyzed by the methods of elemental analysis, BET and TG-MS. The results showed that the catalyst deactivation rate was notable at the beginning of run, and then gradually reached a steady state after 448 h. In the initial period the catalyst deactivation may mainly be caused by the formation of the carbon deposits. The carbon deposits blocked the catalyst pores and the accessibility of active center decreased. The TG-MS analysis identified three types of carbon species deposited on the catalysts, viz.: the low temperature carbon deposit with high H/C atomic ratio, the medium temperature carbon deposit, and the high temperature carbon with low H/C atomic ratio. The amount of high temperature carbon deposits on the catalyst determined the overall activity and, therefore the high temperature carbon was a major contributor to the deactivation of Ni-Mo-W catalyst.
What problem does this paper attempt to address?