Deactivation of Ni Catalysts During Methane Autothermal Reforming with CO2 and O2 in a Fluidized-Bed Reactor

Zhaoyin Hou,Jing Gao,Jianzhong Guo,Dan Liang,Hui Lou,Xiaoming Zheng
DOI: https://doi.org/10.1016/j.jcat.2007.06.023
IF: 7.3
2007-01-01
Journal of Catalysis
Abstract:A series of different-sized Ni catalysts (4.5–45.0 nm) were prepared and used for methane autothermal reforming with CO2 and O2 in a fluidized-bed reactor. It was found that the activity and stability of Ni catalysts depend strongly on the particle size and the operating space velocity. Small sized Ni is more active and stable at space velocity <54,000 h−1. Characterizations disclosed that methane decomposition rate decreases with the enlarging Ni particle size, and some of the surface carbons (derived from methane decomposition) are inactive in CO2 atmosphere. As the methane decomposition rate slows on larger Ni particles and at higher space velocity to ensure complete conversion of the oxygen, surface Ni will be gradually oxidized by remaining O2, leading to Ni deactivation.
What problem does this paper attempt to address?