Flash joining of 3YSZ and 430 SS using Ag–CuO filler

Yue Cao,Guo-Cheng Xu,Ping Shen
DOI: https://doi.org/10.1016/j.ceramint.2021.10.187
IF: 5.532
2022-02-01
Ceramics International
Abstract:Conventional reactive air brazing (RAB) of stainless steel (SS) to ceramic components usually encounters Cr oxidation and joint embrittlement problems due to high temperature and long dwelling time. Herein, 3 mol% yttria-stabilized zirconia (3YSZ) and 430 SS were joined using an Ag–CuO filler in seconds at relatively low temperatures (875 °C–1050 °C) with the assistance of a direct current passing through the seam. The applied current promoted the melting of the filler and rapid filling of the gap due to Joule heating effect. Also, it facilitated atomic/ionic transport and interfacial reaction. Key joining parameters including current density, joining time and furnace temperature were investigated, and a maximum joint strength of 158 ± 9 MPa was achieved at a current density of 4 A/cm2 for 30 s at 950 °C, which is approximately 50% higher than that of the RAB joints. The formation of AgCu4Zr and Zr-rich intermetallic phases at the 3YSZ/Ag and Ag/430 SS interfaces, respectively, together with the suppression of the growth of Cr-containing oxide, was responsible for the robust joining.
materials science, ceramics
What problem does this paper attempt to address?