Progress in Developing ITER and DEMO First Wall Technologies at SWIP

J. M. Chen,X. Liu,P. H. Wang,P. Huang,J. B. Wang,L. Z. Cai,F. Y. Jin,X. B. Zhu,Q. Li,Y. Y. Chen,Z. X. Wei,M. Xu,X. R. Duan
DOI: https://doi.org/10.1088/1741-4326/ab483a
IF: 3.3
2019-01-01
Nuclear Fusion
Abstract:The first wall (FW) is key component for ITER and the Chinese DEMO—the China Fusion Engineering Test Reactor (CFETR). It faces burning plasma and has a high heat flux (HHF) surface load. Critical issues and key technologies for manufacturing the ITER and CFETR FW are discussed with regards to thermal fatigue performance, Be/CuCrZr and W/reduced activation ferritic/martensitic (RAFM) steel bonding, material properties and failure mechanisms. Design improvement of the hypervapotron cooling channel and the joint interface structure was done, which increases the thermal fatigue lifetime of the enhanced heat flux (EHF) ITER FW by more than one order of magnitude as indicated by thermo-mechanical analysis. Small mock-ups and full-size EHF FW fingers were manufactured by qualified technologies in sequence. An HHF test of the small mock-ups showed that Be tile size and defects at the Be/CuCrZr interface have a great effect on the fatigue lifetime. Manufacturing tests showed a thick oxygen-free Cu interlayer could provide a good solution for the interface cracking issue. An ITER EHF FW semi-prototype was manufactured with additional two full-size finger pairs that successfully survived the demanding HHF test at 4.7 and 5.9 MW m−2. Various manufacturing technologies for joining W/RAFM steel for the CFETR FW have been studied, including a TiN coating at the interface as a tritium permeation barrier. Hot iso-static pressed W/RAFM steel joints showed a higher bonding strength than brazing joints but varied a lot with the interlayer metals. Further studies are required to optimize the technologies.
What problem does this paper attempt to address?