Effect of Zn-brazed-interface on Microstructures and Mechanical Properties of Dissimilar 2A12/AZ31 Alloys Friction Stir Lap Welds

Huaibo Deng,Yuhua Chen,Timing Zhang,Shanlin Wang,Limeng Yin,Jilin Xie
DOI: https://doi.org/10.1016/j.matlet.2019.126543
IF: 3
2019-01-01
Materials Letters
Abstract:To improve the mechanical behavior of dissimilar Al/Mg joints, Zn foil, as a brazing filler, was added to the Al/Mg interface when conducting friction stir lap welding with 2A12/AZ31 alloys. Results showed that new phases, such as Mg0.97Zn0.03, Al(0.403)Zn(0.597 )and MgZn2, rather than the continuous brittle Al12Mg17 intermetallic compound (IMC), are formed in the brazing area. At a rotation speed of 375 rpm and a travel speed of 30 mm/min, the tensile shear load of the hybrid joint reached 5.5 kN through a Zn-brazed interface, thereby preventing the formation of the continuous brittle IMC Al12Mg17 and enlarging the overlap bonding area. (C) 2019 Elsevier B.V. All rights reserved.