Effect of Intermediate Layer on Microstructure and Mechanical Properties of Ti/Al Joint Welded by Friction Stir Welding

Zhang Xin,Chen Yuhua,Wang Shanlin
2016-01-01
Rare Metal Materials and Engineering
Abstract:Ti/Al joints were fabricated by friction stir welding (FSW) 3 mm thick 2A14 aluminium alloy and TC4 titanium alloy with Zn and Ni ribbons of 0.05 mm thickness as intermediate layer. Effects of Zn and Ni on the microstructure and mechanical properties of the joints were studied. The results indicate that the tensile strength of the joint with Zn is up to 237.3 MPa, nearly 56.7% of that of the aluminum alloy when the welding velocity is 75 mm/min and the rotation speed 375 r/min. Under the same processing parameters, the tensile strength of the joint with Ni as intermediate layer reaches 285.3 MPa, nearly 68% of that of the aluminum alloy. Ni as intermediate layer can reduce brittle phase TiAl3, and the fracture mode is brittle/ductile fracture.