Abstract:Two kinds of SiC coatings were fabricated on C/C composites by a two-step pack cementation. The CS-SiC coating was prepared using Si, graphite and Al2O3 powder as the raw materials, while the raw materials of FCS-SiC coating were composed of Si, graphite, Al2O3 and β-SiC powder. The morphology and phase composition of the coatings were characterized by scanning electron microscopy and X-ray diffraction. The results showed that the FCS-SiC coating possessed a denser surface with smaller grain sizes. Meanwhile, some large open-holes and penetrating cracks could be found in the surface of the FCS-SiC coating. The oxidation and thermal properties of the coatings were investigated and compared. After oxidation at 1773K for 43h, the FCS-SiC and CS-SiC coating presented a weight-loss of 0.64% and a weight-gain of 0.44%, respectively. The FCS-SiC coating showed a weight-loss of 0.52% after 30 thermal cycles between 1773K and room temperature, while the CS-SiC coating exhibited a weight-gain of 0.11% after 50 thermal cycles. The inferior protection ability of the FCS-SiC coating could be attributed to the severe defects. These severe defects were formed in the preparation process of the FCS-SiC coating, which might be ascribed to the effect of the β-SiC additive.
What problem does this paper attempt to address?