Effects of Microwave-Assisted Annealing on the Structure and Magnetic Properties of (nd0.75pr0.25)9fe72ti1zr3mn X Mo4−x B10.5C0.5 Amorphous Ribbons

Tianpeng Wang,Tian,Song Ding,Zhanyong Wang,Qixiao Ni,Ding Zhou,Guangle Dong,Yanli Sui,Minglin Jin
DOI: https://doi.org/10.1007/s10948-017-4448-z
2017-01-01
Journal of Superconductivity and Novel Magnetism
Abstract:The amorphous as-spun ribbons with nominal composition (Nd0.75Pr0.25)9Fe72Ti1Zr3Mn x Mo4−x B10.5C0.5(x = 1, 2, 3) were annealed by microwave-assisted annealing. The effects of the Mn-doped alloys on glass-forming ability (GFA), crystallization, and magnetic properties of the Nd2Fe14B/α-Fe nanocomposite magnets were examined by thermal differential scanning calorimetry (DSC), X-ray diffraction (XRD), and vibrating sample magnetometry (VSM). An appropriate amount of Mn was beneficial to the optimization of the structure and magnetic properties. Compared with conventional annealing, the microwave-assisted annealing has contributed to the precipitation of hard magnetic phases and adjusted the proportion of hard and soft magnetic phases. The optimum magnetic properties with coercivity up to 805 kA/m were found for ribbons (with composition x = 1) annealed under the microwave power of 2000 W for 10 min.
What problem does this paper attempt to address?