Differences in the Structure and Magnetic Properties of (nd0.75pr0.25)(9.5)fe76x4b10.5 (x=nb, Zr) Ribbons by Conventional and Microwave-Assisted Annealing Treatment

Sui Yanli
DOI: https://doi.org/10.1016/s1002-0721(17)60961-x
IF: 4.632
2017-01-01
Journal of Rare Earths
Abstract:Amorphous ribbons with (Nd0.75Pr0.25)9.5Fe76X4B10.5(X=Nb, Zr) nominal composition were annealed by conventional and microwave-assisted annealing furnaces, respectively. The thermal decomposition process, structure and magnetic properties of products were characterized by a thermal differential scanning calorimeter (DSC), X-ray diffraction (XRD) and a vibrating sample magnetometer (VSM). The addition of Nb and Zr increased the glass-forming ability (GFA) of as-spun ribbons. The proportion of Nd2Fe14B and α-Fe could be adjusted with power from 800 to 2000 W in microwave annealing process, during which the well-coupling between the soft and hard magnetic phase and higher coercivity reached up to 780.2 and 815.4 kA/m for (Nb,Zr)-doped alloys. The best magnetic properties of ribbons could be obtained by annealing at 650 °C for 10 min under the microwave power of 2000 W.
What problem does this paper attempt to address?