Surface modification of carbon fiber and preparation of hydroxyapatite coating
Li ZHANG,Xue-ni ZHAO,Xu-dong WANG,Wan-ying WANG,Jing ZHANG,Jian-jun YANG,Fu-zhen HE,Ke YANG,Jun-peng LIU
DOI: https://doi.org/10.19481/j.cnki.issn2096-398x.2017.05.014
2017-01-01
Abstract:In this study ,the carbon fiber (CF) was modified by concentrated HNO3 ,and the hydroxyapatite (HA ) coating with uniform morphology was prepared by electrochemical deposition on the surface of CF before and after HNO3 modification .The microstructure and phase composition of the coating were characterized by scanning electron microscopy (SEM ) and X-ray diffraction (XRD) ,respectively .The results show that the deposition products on CF are HA ;After being modified by concentrated HNO3 ,the deposition mass of HA coating increase obviously ,and the morphology is more uniform and dense;With the increase of dep-osition current ,the deposition mass of the coating first increased and then decreased ,w hen the current is 5 mA ,the deposition mass reaches the maximum about 2 .7 mg ,and grain grad-ually changed from needle to sticks;With the increase of deposition time ,the deposition mass of the coating gradually increased ,w hen the deposition time is 2 h ,the deposition mass rea-ches the maximum 3 .6 mg .