Microstructure and mechanical analysis of W/P91 steel HIP-joint with Ti interlayer

Jichao Wang,Wanjing Wang,Z. Sun,X. Y. Wang,Ran Wei,Chunyi Xie,Qiang Li,Guang-Nan Luo
DOI: https://doi.org/10.1016/j.fusengdes.2016.07.012
IF: 1.905
2016-01-01
Fusion Engineering and Design
Abstract:•W and P91 steel can be joined successfully using the Hot Isostatic Pressing (HIP) method with Ti interlayer.•The experiment was conducted at 760°C below the P91 steel austenitizing temperature with the pressure 150MPa for 4h.•The residual stress concentration is responsible for the fracture of HIP joints under low joining temperature.•Low temperature can reduce the reaction products and improve the mechanical properties of W/Ti/P91 steel joints.
What problem does this paper attempt to address?