Crystal structure, phase content, and tensile properties of As-cast Mg–Gd–Y–Al alloys
Xiqin Liu,Fang Liu,Zili Liu,Huanjian Xie,Jian Li
DOI: https://doi.org/10.1016/j.mtcomm.2020.101286
IF: 3.8
2020-12-01
Materials Today Communications
Abstract:<p>The lattice parameters, phase content, and tensile properties of as-cast Mg–<em>x</em>Gd–(4–<em>x</em>)Y–2Al (<em>x</em> = 0, 2, 4) alloys were investigated via X-ray diffraction, Rietveld refinement, scanning electron microscopy, and transmission electron microscopy. The Mg-RE phase, Al<sub>2</sub>RE phase, and Al<sub>11</sub>RE<sub>3</sub> phase occurred in all three alloys. Furthermore, the cell volume and axial ratio (<em>c/a</em>) of the α-Mg matrix decreased with increasing (0–4 wt.%) Gd content. The abundance of the Al<sub>2</sub>RE and Mg-RE phases decreased with increasing Gd content, whereas that of the Al<sub>11</sub>RE<sub>3</sub> phase increased. Moreover, Al<sub>2</sub>RE particles formed at the grain centers served as active nucleation sites, thereby leading to grain refinement, and acicular Al<sub>11</sub>RE<sub>3</sub> phases restricted the growth of α-Mg. The tensile properties improved with increasing Gd content. In fact, the optimal mechanical properties (yield strength: 77.83 MPa, ultimate tensile strength: 195.01 MPa, and elongation: 15.71 %) were obtained for the Mg–4Gd–2Al alloy. Furthermore, strengthening of the material occurred mainly via second-phase strengthening and solid-solution strengthening. Block Al<sub>2</sub>RE particles can cut the matrix during the stretching process, and the acicular Al<sub>11</sub>RE<sub>3</sub> phase may play a major role in enhancing the tensile properties. In addition, the ductility of the alloy system improved with decreasing axial ratio (<em>c/a</em>).</p>
materials science, multidisciplinary