Surface Modifications of W Divertor Components for East During Exposure to High Heat Loads with He

C. Li,H. Greuner,Y. Yuan,S. X. Zhao,G. N. Luo,B. Boeswirth,B. Q. Fu,Y. Z. Jia,X. Liu,W. Liu
DOI: https://doi.org/10.1016/j.jnucmat.2014.10.063
IF: 3.555
2015-01-01
Journal of Nuclear Materials
Abstract:Flat-type W/Cu plasma-facing components have been developed for the new generation divertor of the Chinese Experimental Advanced Superconducting Tokamak. Surface modifications of such actively water-cooled W components following short and long pulse high heat loading coupled with He particle loads with fluence of 3×1022m−2 have been investigated. An adiabatically loaded W block was investigated as a comparison and exposed to short pulse loads. Blistering was observed on all sample surfaces, but was less pronounced on the components than on the W block, due to the significant lower surface temperature caused by active cooling. For components, longer pulse loads gave rise to a rougher surface. Furthermore, most blisters on components are found to be less than 1μm in diameter, with just a very few blisters larger than 1μm, observed only in some near 〈111〉 grains.
What problem does this paper attempt to address?