Surface Modification of W–V Alloy Exposed to High Heat Flux Helium Neutral Beams

Jun Wang,Chun Li,Yue Yuan,Henri Greuner,Long Cheng,Guang-Hong Lu
DOI: https://doi.org/10.1088/1741-4326/aac72c
IF: 3.3
2018-01-01
Nuclear Fusion
Abstract:Surface modification of tungsten vanadium (W-V) alloy under high heat flux helium particle bombardment has been studied. W-5 wt.% V samples were irradiated by repeated helium pulses at a peak surface temperature of 900 C-degrees and 1800 C-degrees, respectively, in the neutral beam facility GLADIS. The effect of helium fluence on the surface morphology changes was investigated by increasing the helium fluence from 1 x 10(22) m (-2)- 2 x 10(22) m(-2). Blistering is the typical structure after the repeated helium pulses loading at 900 C-degrees, and it becomes more severe with increased fluence. A porous structure becomes dominant at 1800 C-degrees. An evolution of a porous structure to coral-like structure is observed as fluence increases. In addition, the three typical regions in the W-5V, W-enriched region, W-V solid solute region, and V-enriched region, exhibit different damage features. The W-V solid solute region shows better surface damage resistance compared to the other two regions.
What problem does this paper attempt to address?