Dependence of Optical Properties of Chemical Bath Deposited SnS[sub 2] Films on Deposition Time

G. Sreedevi,K. T. Ramakrishna Reddy
DOI: https://doi.org/10.1063/1.4791224
2013-01-01
AIP Conference Proceedings
Abstract:SnS2 films were grown on glass substrates by chemical bath deposition by varying the deposition time from 3 hr. to 6 hr. The influence of deposition time on the morphological and optical properties of these films was studied from scanning electron microscopy (SEM) and optical transmittance measurements. The films had granular surface morphology without any voids or cracks that became denser with the rise of deposition time. The optical studies revealed direct allowed optical transition for the films and the evaluated energy band gap varied in the range of 2.81 - 2.98 eV. The refractive index and extinction coefficient of the layers were also calculated.