LLDPE Modified by Ultraviolet Irradiation and Toughening of PA66

RAN Qianping,HUA Hongyan,WU Shishan,SHEN Jian
DOI: https://doi.org/10.3321/j.issn:1000-3851.2006.02.008
2006-01-01
Abstract:Some oxygen containing groups such as C—O,CO and —OH were introduced onto the molecular chains of linear low-density polyethylene(LLDPE) through ultraviolet irradiation in air without other additives and chemical pollution.These groups contents increase with the ultraviolet irradiation time.After the ultraviolet irradiation,the crystal shape and distance of the crystal plane of LLDPE remain unchanged.However,the melting temperature and crystallinity decrease.Compared with those of LLDPE/nylon66(PA66) composites,the dispersion of irradiated LLDPE in irradiated LLDPE/PA66 composites and the compatibility between irradiated LLDPE and PA66 and interfacial interaction are improved obviously.The mechanical properties of irradiated LLDPE/PA66 composites initially increase and then decrease with increasing the irradiation time.Their maximums are obtained when the irradiation time was 24 h.The tensile strength,bending strength and notched impact strength of irradiated LLDPE for 24h/PA66 composites increase by about 20%,13% and 330% compared with those of LLDPE/PA66 composites;the irradiated LLDPE shows higher toughening effect.
What problem does this paper attempt to address?