Preparation of Hydrophobic SiO2 Aerogels at Ambient Pressure

Yi-min CHEN,Kai XIE,Xiao-bin HONG,Jia-yu XIAO
DOI: https://doi.org/10.3969/j.issn.1001-2486.2005.02.003
2005-01-01
Abstract:The alcogel prepared by sol-gel process of polydiethoxysiloxane (PDEOS) according to the mass ratio of PDEOS:HF:H2O = 20:10:3:0.5, was modified by methyltriethoxysilane (MTES) and washed with alcohol and n-hexane. The obtained gel was then dried under ambient pressure to prepare hydrophobic SiO2 aerogel. It is shown that hydrophobic SiO2 aerogels can be obtained when the mass ratio of MTES/PDEOS is higher than 1.2. The contact angle between hydrophobic SiO2 aerogels and water is larger than 110°, the densities and specific surface areas of hydrophobic SiO2 aerogels are in the range of 125-160 kg/m3 and 560-900 m2/g respectively.