INFLUENCE OF ALUMINA MODULUS AND LIQUID PROPERTIES ON BURNING PROCESS OF TRICALCIUM SILICATE-RICH PORTLAND CLINKERS

郭随华,陈益民,管宗甫,秦守婉,韦江雄,唐润荣,周瑾
DOI: https://doi.org/10.3321/j.issn:0454-5648.2004.03.025
2004-01-01
Abstract:The liquid properties variation caused by alumina modulus(IM) and their influence on burning process and microstructures of tricalcium silicate(C_(3)S)-rich portland clinkers were investigated. The results show that the burnability of clinkers with high silica modulus(SM) and high IM are better than that of clinkers with low SM and low IM at the same C_(3)S content and the high burning temperatures over 1 400 ℃. The increase of IM in the clinker with high SM can raise liquid phase content in the clinker and accelerate the formation of alite. However, the increase of IM in the clinker with low SM results a higher viscosity of the liquid phase during the burning, and retrain the formation of C_(3)S. The number of C_(3)A crystals in the clinker is larger when the IM value is higher than 1.68. The number of C_(4)AF crystals in the clinker with SM=3.00 is the largest when IM value lies in the range of 1.6~1.8. The sizes of alite in the clinker decrease, the ratios of length to breadth of alite increase remarkably and there are much more inclusions in the alite when the IM value of the clinker increases in the range of 1.0~1.9.
What problem does this paper attempt to address?