Influence and mechanisms of active silica in solid waste on hydration of tricalcium aluminate in the resulting composite cement

Dapeng Zheng,Hongzhi Cui,Waiching Tang,Guochen Sang,Tommy Y. Lo
DOI: https://doi.org/10.1016/j.mtcomm.2021.102262
IF: 3.8
2021-06-01
Materials Today Communications
Abstract:<p>Many industrial solid wastes are rich in silica (SiO<sub>2</sub>) which can be used as supplementary cementitious material (SCM) to replace part of Portland cement. Existing studies mainly focus on the impact of solid waste on tricalcium silicate (C<sub>3</sub>S) hydration. Since tricalcium aluminate (C<sub>3</sub>A) is the most reactive component of the Portland cement, it is of great interest t to investigate the effect of solid waste containing SiO<sub>2</sub> on the hydration process of C<sub>3</sub>A. In this study, different amounts of nano-silica (nano-SiO<sub>2</sub>) were mixed with C<sub>3</sub>A and the hydration products after 72 hours of hydration were analyzed by means of X-ray diffraction (XRD), Fourier Transform Infrared analyzer (FT-IR), Environment Scanning Electronic Microscope - Energy Dispersive Spectrometer (ESEM-EDS), X-ray Photoelectron Spectroscopy (XPS) and Solid-state Nuclear Magnetic Resonance (NMR). The results showed that nano-SiO<sub>2</sub> can promote the hydration of C<sub>3</sub>A and stabilize the hydration products of C<sub>3</sub>A in the form of crystalline hydrogarnet (C<sub>3</sub>AH<sub>6</sub>). The formation of Si-O-Al bonds was also found in the hydration products. ESEM results revealed that the surface of the crystalline hydration products (C<sub>3</sub>AH<sub>6</sub> particles) was covered by gel-like products. The results from the XPS and NMR analyses further confirmed that the negatively charged nano-SiO<sub>2</sub> and the silicate anions can literally interact with C<sub>3</sub>A to produce calcium silicoaluminate hydrate (C-A-S-H) gel, whereas the formation of C-A-S-H is attributed to the substitution reaction of Al in the Si-O-Si network occurring on the surface of C<sub>3</sub>A. In addition to the reactive silica-aluminum component reacting with Ca(OH)<sub>2</sub> to form additional calcium silicate hydrate (C-S-H) and C-A-S-H gels, the reactive silicon in solid waste can also undergo pozzolanic reaction with C<sub>3</sub>A to form C-A-S-H gel.</p>
materials science, multidisciplinary
What problem does this paper attempt to address?