Removal of Nickel from Spent Electroless Nickel-Plating Bath with Nickel Foam Cathode

于秀娟,郑彤,魏杰,周定
DOI: https://doi.org/10.3969/j.issn.1005-9113.2002.04.002
2002-01-01
Abstract:The electrochemical method was used to remove nickel ion from spent electroless nickel plating bath(pH = 5.3). An electrolytic cell was composed of a porous nickel foam cathode and an inert RuO2/Ti anode.Nickel ions were reduced and deposited on the surface of the nickel foam cathode. The effect of current density(i), linear velocity of wastewater (v), gap between cathode and anode (dc/A) and reaction time (t) on nickelremoval rate and current efficiency were studied. As reaction time prolonged, nickel removal rate increasedwhile current efficiency decreased. And larger v and smaller dc/A can enhance nickel removal rate and increasecurrent efficiency by promoting mass transfer and dropping concentration polarization. The effect of current den-sity on nickel removal by electrochemistry was related to other parameters. After three hours' electrolysis withi = 1.0 A/dm2, v = 18.5 cm/min and dc/A = 0. 5 cm, nickel removal rate and current efficiency reached85.6% and 29. 1%, respectively.
What problem does this paper attempt to address?