Spark plasma sintering of TiC ceramic with tungsten carbide as a sintering additive

Lixia Cheng,Zhipeng Xie,Guanwei Liu
DOI: https://doi.org/10.1016/j.jeurceramsoc.2013.04.017
IF: 5.7
2013-01-01
Journal of the European Ceramic Society
Abstract:By adding a small amount of tungsten carbide (WC) as sintering aids, nearly fully dense TiC ceramics were obtained by spark plasma sintering at 1450–1600°C. The results show that the densification temperature of TiC ceramic was significantly decreased with the addition of 3.5wt% WC. Compared with the monolithic TiC, the densification temperature of TiC–3.5wt% WC is lower by ∼150°C and no deterioration of mechanical properties is observed. The TiC composite sintered at 1600°C exhibits full density, a Vickers hardness of 28.2±1.2MPa, a flexural strength of 599.5±34.7MPa and a fracture toughness of 6.3±1.4MPam1/2.