Preparation of Ni-diamond composite coating by composite electroplating

WANG Meijuan,WANG Richu,PENG Chaoqun,FENG Yan,ZHANG Chun,DENG Lijie
2013-01-01
Abstract:The Ni-diamond composite electrodeposition was prepared by composite electroplating when diamond particles with a diameter of 40 μm were put into the solution of Ni electroplating. The effects of temperature, pH value of solution, concentration of Ni2+, cathode current density and concentration of diamond particles on the quality of Ni-diamond composite coatings were investigated by the cathodic potentiodynamic polarization, SEM and microhardness tester. The optimized technological conditions of Ni-diamond composite electrodeposition were obtained. The structure of optimized Ni-diamond composite coating was tested by XRD. The experimental results show that the optimized technological conditions are: NiSO4·6H2O, 132 g/L; NiCl2, 15 g/L; H3BO3, 30 g/L; temperature, (50±1)°C; pH, 3-4; cathode current density, 4 A/dm2; concentration of diamond particles, 30 g/L. The results of SEM indicate that the surface of the Ni-diamond composite coating containing 62.7% diamond particles is neat, and small homogeneous grains are obtained. In comparison with pure Ni coating, the grains of the Ni-diamond composite coating are obviously refined.
What problem does this paper attempt to address?