Zr 1− X Yb X WMoO 8− X /2 ( X = 0, 0.04) Ceramics Fabricated by in Situ Synthesis from Trigonal Polymorph: Preparation, Sintering Process, and Negative Thermal Expansion Properties

Ruiqi Zhao,Xi Chen,Hui Ma,Xishu Wang,Xinhua Zhao
DOI: https://doi.org/10.1007/s10853-012-6698-2
IF: 4.5
2012-01-01
Journal of Materials Science
Abstract:In this study, negative thermal expansion (NTE) Zr1−x Yb x WMoO8−x/2 (x = 0, 0.04) ceramics were fabricated by in situ synthesis from trigonal polymorphous precursors for the first time. Phase transition was studied by means of powder X-ray diffraction. Study on the sintering process of Zr1−x Yb x WMoO8−x/2 (x = 0, 0.04) ceramics was performed by calcining a series of precursor pellets at 950, 980, and 1000 °C for different times, varying from 1 min to 1 h. The results indicate that the sintering process can be mainly divided into three stages: phase transition from trigonal precursors to cubic Zr1−x Yb x WMoO8−x/2 (c-Zr1−x Yb x WMoO8−x/2, 0–5 min), densification of c-Zr1−x Yb x WMoO8−x/2 (6–30 min), and the final sintering stage with little densification (>30 min). Densification reaches almost the maximum in the duration of ~30 min at assigned temperature. Temperature has little influence on densification of ZrWMoO8, but improves that of Zr0.96Yb0.04WMoO7.98 evidently. In addition, densification of ZrWMoO8 can be promoted markedly by introduction of Yb3+.
What problem does this paper attempt to address?