Abstract:In this work, phase pure Cr2AlC and impure Cr2AlC with Cr7C3 have been fabricated to investigate the mechanical, thermal, and electrical properties. The thermal expansion coefficient is determined as 1.25 x 10(-5) K-1 in the temperature range of 25-1200 degrees C. The thermal conductivity of the Cr2AlC is 15.73 W/m K when it is measured at 200 degrees C. With increasing temperature from 25 degrees C to 900 degrees C, the electrical conductivity of Cr2AlC decreases from 1.8 x 10(6) Omega(-1)m(-1) to 5.6 x 10(5) Omega(-1)m(-1). For the impure phase of Cr7C3, it has a strengthening and embrittlement effect on the bulk Cr2AlC. And the Cr2AlC with Cr7C3 would result in a lower high-temperature thermal expansion coefficient, thermal conductivity, specific heat capacity and electrical conductivity. (C) 2011 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?