The effect of milling time and heat treatment on the synthesis of the Cr2AlC MAX phase

Bahman Mansouri,Mahdi Rafiei,Iman Ebrahimzadeh,Farid Naeimi,Masoud Barekat
DOI: https://doi.org/10.1080/00084433.2023.2251210
2023-08-30
Canadian Metallurgical Quarterly
Abstract:Synthesis of the Cr 2 AlC MAX phase was investigated by mechanical alloying. Cr, Al, and C powders were milled and heat treated at temperature range of 500–1300°C for 1 h. X-ray diffraction and differential thermal analysis were used to study the reaction mechanisms and a scanning electron microscope was used to observe the microstructures. The Cr 7 C 3 and Cr–Al compounds were formed by reactions among the initial elements. These compounds transformed to the Cr 2 AlC phase by increasing the temperature. The maximum amount of Cr 2 AlC phase was equal to 97.23 wt.%, which was related to the sample with 45 h of ball milling and subsequent heat treatment at temperature of 700°C. DTA results showed a major exothermic peak at about 685°C, which represents the formation of the Cr 2 AlC . This indicates that most conversions are completed in a single stage, below the temperature of 800°C.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?