Influence of Electrospark Deposition Processes on Thickness of TiC Deposition Coating

LUO Cheng,DONG Shijie,XIONG Xiang
DOI: https://doi.org/10.3321/j.issn:1005-023x.2007.12.036
2007-01-01
Abstract:In order to improve the life of spot-welding electrode for zinc-coated steel,electrospark deposition(ESD) processes were studied taking TiC as fusing material and CrZrCu as spot-welding electrode.ESD parameters(such as capacitance,deposition time,electrode rotate speed and vibratory frequency) pre-treatment as well as post-treatment of the substrate were investigated by means of orthogonal experiment.The results indicate that the capacitance is the most important factor that influences the thickness of ESD TiC coating,the vibratory frequency is less important,the rotate speed of electrode and the depositing time influence slightly.The optimized parameters under the test conditions are capacitance 30 000μF,electrode rotate speed 1 320r/min,vibratory frequency 50Hz,depositing time 120s.Pre-treatment to improve the interface between coating and substrate has a weak influence on the thickness of the coating.Post-treatment(annealing at 700℃×30 min after deposition) can promote elements diffusing and decreases the thickness of the deposition coating.
What problem does this paper attempt to address?