The Propertied Of Ysz Electrolyte Sintering At 1300 Degrees Enc

Minfang Han,Xiuling Tang,Wu Shao
DOI: https://doi.org/10.1007/s11595-007-6775-6
2008-01-01
Abstract:The properties of yttria stabilized zirconia(YSZ) related to the sintering process were discussed. YSZ nano-powders about 40-100 run as raw material, the sub-micrometer grain sizes such as 0.4-3 mu m in YSZ were gotten by sintering process at 1300 degrees C, which was perforined at 1000 degrees C for2 h, then raised the temperat Lire attherateof 50 VA to 1400 degrees C, then decreased directly to 1300 degrees C in 30 minutes, finally at 1300 degrees C for 5-20 hours. The ratio of bigger grain size becornes largeras the holding time increasing at 1300 degrees C. The grains less than I pin areabout 50%, eg, 43.2%, 52.2% and 51. 1 % related to 1300 degrees C holding 5 hours, 8 hours and 10 hours, respectively. As YSZ grain size became small, the electrical conductivities did not decrease, even increased, about 0.20 s/cm at 1000 degrees C. The reduced sintering temperature and time were benefited to co-fire with the electrodes in electrode-supported SOFCs.
What problem does this paper attempt to address?