Hydrothermal and wet-chemical synthesis of pure LiTaO3 powders by using commercial tantalum hydroxide as starting material

Feifei Zheng,Hong Liu,Duo Liu,Shuhua Yao,Tao Yan,Jiyang Wang
DOI: https://doi.org/10.1016/j.jallcom.2008.10.159
IF: 6.2
2009-01-01
Journal of Alloys and Compounds
Abstract:We report here the successful synthesis of lithium tantalate (LiTaO3, IT) powders by using a combined hydrothermal and wet-chemical technique. This synthesis method involves only inexpensive, nontoxic raw materials, such as tantalum hydroxide (Ta(OH)(5)) and lithium carbonate (Li2CO3). Ta(OH)(5) was first dissolved in hydrochloric acid through a hydrothermal process, followed by addition of citric acid (CA) to form stable Ta-CA complex. After pH adjustment with ammonia and addition of Li2CO3, pure IT powders were obtained by calcination at 720 degrees C for 2 h. Compositional, microstructural, and morphological aspects of the final product were evaluated with X-ray diffractometry (XRD) and scanning electron microscopy (SEM). Thermal behaviors and the calcination temperature were determined by thermal analysis. (c) 2008 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?