Sinterability and Piezoelectric Properties of (k,na)nbo3ceramics with Novel Sintering Aid

M Matsubara,T Yamaguchi,K Kikuta,S Hirano
DOI: https://doi.org/10.1143/jjap.43.7159
IF: 1.5
2004-01-01
Japanese Journal of Applied Physics
Abstract:K4CuNb8O23 (KCN) as a sintering aid. The sinterability and electrical properties of KNN ceramics were investigated as a function of KCN concentration. The density of KNN ceramics increased monotonically with increasing the KCN contents, and reached the highest value of 4.40 g/cm(3) with the addition of 0.5 mol% KCN. This is due to the formation of liquid phase, which significantly promotes the densification of KNN ceramics. The Curie temperature (T-c) of pure KNN ceramics was 420degreesC and decreased with increasing the KCN content. With the addition of 0.5 mol% KCN, planar mode electromechanical coupling factor (k(p)) and mechanical quality factor (Q(m)) of KNN ceramics also reached the highest values of 0.39 and 1200, respectively. The KNN ceramics prepared with 0.5 mol% KCN exhibited a large field-induced strain of 0.09% at 40 kV/cm and the piezoelectric constant d(33) of 180 pm/V.
What problem does this paper attempt to address?