Nickel base superalloy GH4049 prepared by powder metallurgy

C.F. Tang,F. Pan,X.H. Qu,B.H. Duan,X.B. He
DOI: https://doi.org/10.1016/j.jallcom.2008.06.038
IF: 6.2
2009-01-01
Journal of Alloys and Compounds
Abstract:The process of preparing nickel base superalloy GH4049 from atomized prealloyed powder is studied. The results show that the compacts with relative density over 99% can be made by sintering at 1350°C for 2h in vacuum. Sintering in vacuum is better than that in argon atmosphere. The sintering way is supersolidus liquid phase sintering. The tensile strength and yield strength and ductility are about 1113MPa and 760MPa and 13% respectively. They are near the wrought superalloy GH4049. There are two kinds of γ′ phase precipitated in the grains. The rectangular γ′ phase is about 200nm and the global γ′ phase is about 40nm. The average grain size is below 80μm. Its property of the compression stress relaxation at 850°C is better than wrought cobalt base superalloy GH605 (L-605). The results lay the foundation of near-net-shape forming for the powder nickel superalloy GH4049.
What problem does this paper attempt to address?