Thermal Stability and Electrode Properties of Melt-Spun Mg65cu25nd10 Amorphous Alloy

L. J. Huang,G. Y. Liang,Z. B. Sun,Y. F. Zhou,D. C. Wu
DOI: https://doi.org/10.1016/j.mseb.2007.06.011
2007-01-01
Abstract:Amorphous Mg-based alloy Mg65Cu25Nd10 was prepared by melt-spinning. Thermal stability and phase transition in the as-quenched alloy were studied by TEM, DSC, X-ray and electron diffraction. It was found that the crystallization process of melt-spun Mg65Cu25Nd10 ribbons consists of three steps. The first crystallization reaction at about 180°C is connected with the formation of Mg2Cu nanocrystalline phase, followed by formation of a coarser grained α-Mg crystalline phase (210–225°C) corresponding to a second crystallization reaction. At higher temperatures a third exothermic effect (at about 320°C) can be detected and the stable Mg2Cu, α-Mg and Cu5Nd phases are present. The electrode properties of the as-quenched and the annealed samples (partially and fully crystallized) were measured and compared as well. The amorphous Mg65Cu25Nd10 alloy shows the highest discharge capacity (430.4mAh/g) and the best life cycle properties in comparison with those of partially crystalline (421.8mAh/g) and almost completely crystallized microstructural states (304.3mAh/g). It was conformed that the discharge capacity is significantly dependent on the composition and microstructure of the electrode materials.
What problem does this paper attempt to address?