Cathodoluminescence of BaAl2O4 Films Co-doped with Tm,Tb and Eu

LOU Zhi-dong,YI Lan-jie,TENG Feng,XU Zheng,YANG Sheng-yi
DOI: https://doi.org/10.3321/j.issn:1000-7032.2007.03.016
2007-01-01
Chinese Journal of Luminescence
Abstract:The most efficient phosphors currently available for fluorescent lamps, cathode-ray tubes, and flat panel displays are sulfides. Recently, there is growing interest in developing thin film oxide phosphors doped with transition metal or rare earth ions because they are chemically and thermally more stable. In addition, it is well known that thin film phosphors have advantages such as high contrast ratio, high ambient visibility, high image resolution and good heat resistance in display applications. For these reasons oxide-based thin film phosphors have been widely studied.In this paper, thin films of barium aluminate (BaAl2O4) doped separately with thulium, terbium, and europium were deposited by a spray pyrolysis method. The effects of preparation conditions on the structural and luminescence properties of the films were investigated. Polycrystalline BaAl2O4 films were formed at an annealing temperature above 700 ℃. Tm3+ and Tb3+ doped films deposited on glass emitted blue and green light, respectively. While in the films doped with europium, both red emission lines from Eu3+ and a broad blue or blue-green emission band from Eu2+ were observed. The BaAl2O4∶ Tm3+ film has the main emission wavelength at 462 nm, and the highest cathodoluminescence (CL) luminance and efficiency at 5 kV and 57 μA/cm2 were 25 cd/m2 and 0.11 lm/W, respectively. For the BaAl2O4∶ Tb3+ film with the main wavelength at 549 nm, the highest CL luminance and efficiency at the same condition were 120 cd/cm2 and 0.55 lm/W, respectively. A luminance of 50 cd/m2 and efficiency of 0.23 lm/W were obtained for red emission at 616 nm of the BaAl2O4∶ Eu3+ film grown on glass. Bright blue emission peaking at 452 nm was obtained in the BaAl2O4∶ Eu2+ film grown on an aluminosilicate ceramic plate and annealed in N2∶H2 (95∶5) at 1 100 ℃. Its luminance and efficiency were 640 cd/m2 and 2.93 lm/W, respectively.
What problem does this paper attempt to address?