Effects of Process Parameters on Electrical Properties of N-Type Bi2Te3 Prepared by Mechanical Alloying and Spark Plasma Sintering

L. D. Zhao,B. -P. Zhang,J. -F. Li,M. Zhou,W. S. Liu
DOI: https://doi.org/10.1016/j.physb.2007.06.009
IF: 2.988
2007-01-01
Physica B Condensed Matter
Abstract:n-Type Bi2Te3 thermoelectric materials were prepared by spark plasma sintering (SPS) using mechanically alloyed powders. Seebeck coefficient and electrical conductivity of the resultant materials were measured, with emphasis on the effects of sintering process parameters on the electrical properties. The power factor was improved from 1.5 to 1.6mW/mK2 when the SPS pressure was increased from 20 to 50MPa at 623K, and was further increased to 2.1mW/mK2 under 50MPa by raising the SPS temperature from 623 to 673K. The maximum power factor was obtained for the sample sintered under optimized SPS process parameters, in which the sintering temperature and the sintering pressure are 673K and 50MPa, respectively.