Influence of Ph Value of Oxidizing Solution on the Microstructure and Magnetic Properties of Ni-Zn Ferrite Films Deposited at Low Temperature

HU Qing-ping,DONG Ze-hua,BAI Ren-liu,SHEN Xiang,FENG Ze-kun,HUANG Dan-feng
DOI: https://doi.org/10.3969/j.issn.1001-3830.2007.03.010
2007-01-01
Abstract:Ni-Zn ferrite films with thickness of 1-2μm were prepared by spin-spray plating method at 90℃ on glass substrates from the deoxidizing solution of FeCl2+NiCl2+ZnCl2 and the oxidizing solution of CH3COONH4+ NH3H2O+NaNO2. XRD pattern shows that the diffraction peaks of the deposited film are corresponding with characteristic peaks of the spinel ferrite. When the pH value of oxidizing solution increases from 8.0 to 8.8, both the deposition rate and surface roughness of the films increase. In addition, the film prepared at the pH value of 8.8 has a chemical composition of Ni 02.+4 3 Zn 02.+0 9 Fe 02.+4 8 Fe 32+ O 4. This film exhibits a large saturation magnetization of 210.3kA/m and low coercivity of 1.218kA/m.Therefore, the film would be applicable to both radio-frequency inductors and wave absorbers for electromagnetic interference suppression.
What problem does this paper attempt to address?